| 机织产品 |
产品名称 |
单纱断裂强度(CN/tex) |
强力(CV%) |
条干(CV%) |
拈度(cm) |
C60s |
13.5 CN/tex |
10.6 |
18.9 |
134/10 |
JT/C 45s 65/35 |
19.3 CN/tex |
9.0 |
14.1 |
90.8/10 |
C40s |
15.6 |
9.9 |
16.0 |
95.8/10 |
T/C 40s 50/50 |
16.7 |
9.7 |
15.5 |
88.3/10 |
T/C 31s 50/50 |
16.6 |
9.0 |
15.2 |
77.4/10 |
C30.5s |
15.2 |
10.1 |
16.1 |
79.5/10 |
C/T 22.5s 70/30 |
14.1 |
8.4 |
14.8 |
68.3/10 |
|
| 针织产品 |
产品名称 |
单纱断裂强度(CN/tex) |
强力(CV%) |
条干(CV%) |
拈度(cm) |
JC60s |
15.5 |
9.8 |
CV%14.5 |
127/10 |
JC40s |
15.2 |
7.9 |
13.5 |
88.6/10 |
|
| 气流纺纱 |
产品名称 |
单纱断裂强度(CN/tex) |
强力(CV%) |
条干(CV%) |
拈度(cm) |
C16s |
10.0 |
|
13.4 |
79/10 |
T/C7.2s |
14.1 |
|
|
31.5/10 |
| 注:C60s
C40s JC40s 各项指标均能达到乌斯特公报统计值5%水平,涤绵混纺纱各质量指标均能达到乌斯特公报统计值25%水平。 |
|
|